What is the proper way to anneal the mouth and neck area of rifle brass.
I would like to hear your method.
What is the proper way to anneal the mouth and neck area of rifle brass.
I would like to hear your method.
I am sitting in my angry chair!
I have a square metal pan I pour some water in the pan about 1/2 inch set up the cases on one end.Turn out the lights,heat the cases until they just turn color and then knock them over in the water with a pencil or wooden dowel.
NRA, TSRA, GUN OWNERS OF AMERICA
BEING THE MODERATOR OF THE ROADHOUSE IS LIKE BEING THE JANITOR OF A PEEP SHOW.
I use a lead melting pot, run the temps on up, and after f.l. resizing, trimming, etc., I take each case, hold it at the case head, and dip it in the molten lead to the point where I want the anneal, and then when my fingers start to get uncomfortable, I move, quickly, to drop the case in a bucket of water, located well below the bench.
The first couple of times you do this you are likely to burn your finger or thumb tips a little bit. I stress: when it starts to get uncomfortable, MOVE! to the water quench.
When stubbicatt says MOVE! he means MMMOOOOOOOOVVVEE!!!!!!!!!!!!!!!!
It goes from warm to hot a lot faster than most people can react.
I pour some water in the pan about 1/2 inch set up the cases on one end.Turn out the lights,heat the cases until they just turn color and then knock them over in the water with a pencil or wooden dowel.
-----------------------------------------
Last edited by slamfire51; 12-31-2010 at 09:55 AM. Reason: SPAM in signature
Hey Shandy - welcome to the board. Please don't take offense at the sig removal - please review the board rules. Looking forward to seeing more posts from you!
~Nemo me impune lacessit~
Yes.
~Nemo me impune lacessit~